MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: PA 66, non-reinforced, injection molding, halogen free flame retardant, improved flowability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.169 g/cc0.04223 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/in60x60x2; 270 °C / WZ 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527-1,-2
Elongation at Yield >= 20 %>= 20 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.50 GPa218 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 55.0 MPa7980 psi2 mm/min; ISO 178-A
Flexural Yield Strength 40.0 MPa
@Strain 3.5 %
5800 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 1.60 GPa232 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 7.8 %7.8 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 8.0
@Frequency 100 Hz
8.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.055
@Frequency 1e+6 Hz
0.055
@Frequency 1e+6 Hz
IEC 60250
 0.20
@Frequency 100 Hz
0.20
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 265 °C509 °F10°C/min; ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding; ISO 294
 260 - 270 °C500 - 518 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® A 30 H3.0 000000 Nylon 66
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25

PLANW9201 / 207994

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.