MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pasargad Polymer Peyvand Pasalac 3P-H9000W ABS/PC
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Form: Pellets

Processing Method: Injection Molding

Uses:

  • Automotive Application
  • Furniture
  • Appliance Components
  • Automotive Exterior Parts
  • Automotive Interior Parts

Information provided by Pasargad Polymer Peyvand Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527-2
Elongation at Break 60 %60 %ISO 527-2
Tensile Modulus 2.80 GPa406 ksiISO 527-2
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 230 °C446 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FUnannealed; ISO 75-2/C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax PC Series™ 300 Paper Ceramic Fiber Filtration Media
Trinseo PULSE™ 2000 ABS + PC
Silberline SilBerCote® PC 8152Z
Polymax® Maxelast® A9970H TPE, ABS/PC Overmold
Polymax® Maxelast® A9830 TPE, ABS/PC Overmold

PPASAR032 / 176120

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.