MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 250 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 250 adhesive is a one-coat adhesive used to bond a variety of elastomers to various substrates during vulcanization of the elastomer. It is composed a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in an organic solvent system. A single coat of Chemlok 250 adhesive will bond compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR), butyl (IIR), EPDM and polyepichlorohydrin (ECO) polymers to a variety of metals. These metals include carbon and alloy steels, stainless steel, aluminum, copper and copper alloys, magnesium and zinc, as well as a variety of plastics, composites and fabrics.

Features: requires only a single coat for most applications, reducing labor, solvent usage, inventory and shipping costs. bonds a wide variety of elastomers to metals, plastics and fabrics; suitable for existing production lines; tolerates a wide variety of stock formulations. provides rubber tearing bonds; provides superior adhesion to plated metals, lowering scrap rates.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.16 g/cc0.0403 - 0.0420 lb/in³
Solids Content 23.5 - 27.5 %23.5 - 27.5 %by weight
Brookfield Viscosity 200 - 550 cP
@Temperature 25.0 °C
200 - 550 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 33.0 °C91.4 °FPensky-Martens
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene, Trichloroethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9080 / 232469

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.