MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP5TC-80 One component thermally conductive, electrically insulating epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Paste consistency
  • Ultra fine particle size filler
  • Superior thermal conductivity
  • Low thermal resistance
Product Description: Master Bond EP5TC-80 is a one component, flowable paste epoxy for bonding, sealing and small encapsulation applications. EP5TC-80 is a special system. A typical, unfilled epoxy is highly electrically and thermally insulative (with a thermal conductivity value of about 0.25 W/(m-K)). Adding filler materials that conduct heat and not electricity, generally increases thermal conductivity (maybe up to 1-2 W/(m-K)). EP5TC-80 is able to achieve up to 3.3-3.7 W/ (m-K). It is shipped at -40°C and should be stored at that temperature. Once removed from the freezer, to obtain the best properties, the material should be used within 12 hours. Any leftover material should be discarded. This system bonds well to a wide variety of substrates such as metals, composites, ceramics and many plastics. It has particularly noteworthy tensile modulus and compressive strength. The filler material has ultra fine particles, with the largest being 10-15 microns, which allows it to be applied in very thin sections. The end result is very low thermal resistance. The combination of fine bond lines and thermal conductivity lowers the thermal resistance to 6-10 x 10-6 K-m2/W. Curing is simple and straightforward, 80°C for 90-120 minutes with an optional post cure of 1-2 hours at 80°C to optimize properties. EP5TC-80 resists water, oils and fuels. It is gray in color. The service temperature range is -50°C to +150°C. With its robust thermal conductivity, it can solve thermal management issues in aerospace, electronic, opto-electronic, and specialty OEM applications. EP5TC-80 is a versatile system which can be used for bonding heat sinks to circuit boards, coils and motors, die attaching in optics, bonding SMDs, potting power modules and encapsulation of very small coils.

Product Advantages:

  • Single component, no mixing needed
  • Flowable, can cure up to 1/4 inch thick
  • Low shrinkage
  • Highly dimensionally stable
  • Passes NASA low outgassing
Best usage within 12 hours after removing from freezer; discard leftover material

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.45 g/cc2.45 g/cc
Solids Content 100 %100 %
Viscosity 60000 - 180000 cP60000 - 180000 cPthixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 90 - 10090 - 100
Tensile Strength 10.3 - 20.7 MPa1500 - 3000 psi
Elongation at Break 0.50 - 1.5 %0.50 - 1.5 %
Tensile Modulus >= 10.3 GPa>= 1500 ksi
Compressive Strength 172 - 186 MPa25000 - 27000 psi
Adhesive Bond Strength 1.72 - 3.10 MPa250 - 450 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.6
@Frequency 60 Hz
4.6
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 3.31 - 3.75 W/m-K23.0 - 26.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 110 - 115 °C230 - 239 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 120 min
@Temperature 80.0 °C
1.50 - 2.00 hour
@Temperature 176 °F
with optional post cure of 1-2 hours at 80°C
Shelf Life 3.00 - 6.00 Month
@Temperature -40.0 °C
3.00 - 6.00 Month
@Temperature -40.0 °F
storage in a freezer
 
Descriptive Properties
Thixotropic index2.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5908 / 306797

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.