Polypropylene random copolymer. Titanpro L-670M is created for extrusion coating on BOPP films which complies with the U.S. Food and Drug Administration (FDA) regulation as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. TSCA Registry: CAS# 9010-79-1 Applications: Heat sealable layer; Quality packaging application Advantages: Low heat sealing temperature; Good bond strength; Excellent gloss and clarity; Good processability Fabrication: Equipment - general extrusion coating line; Techniques - standard processing Information provided by Lotte Advanced Materials. |