MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CHT QGel 303 Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: QGels are addition-cure clear, soft, moderately cross-linked silicone polymer. Silicone gels provide protection from moisture, vibration, thermal, or mechanical shock.

Key Features

  • Soft gel
  • 1:1 mix ratio
  • Fast 9-minute gel time at room temperature

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccA; BS ISO 2781
 0.970 g/ccB; BS ISO 2781
Brookfield Viscosity 700 cPA
 750 cPB
Storage Temperature <= 38.0 °C
 
Mechanical PropertiesOriginal ValueComments
Penetration 4.0 - 8.0[mm], 19.5g Cone Weight
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D-257
Dielectric Constant 2.8ASTM D-150
Dielectric Strength >= 500 V/mil
Dissipation Factor 0.0010ASTM D-150
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43
 1.43
@Wavelength 589 nm
Transmission, Visible 89.95 %
@Thickness 1.00 mm,
Wavelength 400 nm
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
 60.0 min
@Temperature 25.0 °C
Gel Time 9.00 min
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceAddition
ColorPurple
Mix Ratio1:1By Weight
RheologyGel
Work life4 minto Double Initial Viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL053 / 314536

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.