MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 718 Synthetic Turf Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Turf-set 718 is a one component, moisture curing, solvent based polyurethane adhesive designed for synthetic turf applications. This adhesive exhibits high “green strength” properties for good wet grab but its uniqueness is due to its inherent superior application properties that allow the adhesive to retain ridges or high points immediately after spreading which aid in the bonding to synthetic turf backings, seam tapes and other non uniform or porous materials. These application properties permit easy field application even under adverse weather conditions.

AW-718 has many uses in bonding; golf surfaces, landscaping surfaces, playgrounds and athletic fields.

Once curing is complete the adhesive develops outstanding heat, water and solvent resistance and will remain flexible in low temperature conditions. Turf-set 718’s unique thixotropy allows this adhesive to spread very easily due to its thinning capabilities. Turf-set 718 has been designed to be used on synthetic turf and synthetic turf seaming fabrics with equal success. The adhesive should be applied with a notched squeegee, notched trowel or knife coating applicator directly after removing from container. Once applied, any high spots made by a trowel-like applicator will remain standing for proper mating of the turf and the seaming material. For best result an open time of 10 – 15 minutes would allow the adhesive to “tack up” aiding in enhancing its wet grab/green strength characteristics. Although the adhesive’s viscosity appears very high it has the property of spreading smoothly and evenly with little effort in all weather conditions.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI925 / 232219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.