MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TechnoCompound TechnoMid 66 1 HWHV Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: High Strength and Stiffness
Very good Impact
High Heat Deflection Temperature
Low Abrasion and good Friction Properties
High Chemical Resistance
Very good Dampening
Very good Flow Properties

Typical Applications:

  • Automotive: Air ducts, oil trays, fan wheels, fasteners, engine covers levers, pedals, seat adjustments, mirror plate
  • Electrical and Electronics: Connectors, Plugs, Coil shell, Circuit breakers
  • Building, Construction: Dowels, Thermal breaks, Bearings, Furniture fittings
  • Sports and Leisure: Ski bindings, Hockey stick, Grommet bands

Information provided by TechnoCompound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 2.5 - 3.2 %2.5 - 3.2 %Humidity; ISO 62
 9.0 - 9.5 %9.0 - 9.5 %ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294
Melt Flow 35 g/10 min
@Load 0.00500 kg,
Temperature 275 °C
35 g/10 min
@Load 0.0110 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 75.0 MPa10900 psi50 mm/min; ISO 527
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527
Tensile Modulus 2.90 GPa421 ksi1 mm/min; ISO 527
Flexural Modulus 2.80 GPa406 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VA; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTECHNO063 / 306425

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.