MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC CYCOLAC™ INP630 ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High heat AMSAN pellets.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Melt Flow  10.9 g/10 min
@Load 3.80 kg,
Temperature 230 °C
10.9 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 21 g/10 min
@Load 10.0 kg,
Temperature 220 °C
21 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Flexural Yield Strength 58.0 MPa8410 psi2 mm/min; ISO 178
 115 MPa16700 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.62 GPa525 ksi2 mm/min; ISO 178
 3.88 GPa563 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.190 J/cm0.356 ft-lb/inASTM D256
 0.130 J/cm
@Temperature -30.0 °C
0.244 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²80*10*4; ISO 180/1A
 1.00 kJ/m²
@Temperature -30.0 °C
0.476 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.100 J/cm²0.476 ft-lb/in²ISO 179/2C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 3.20 mm
230 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C210 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 116 °C241 °FRate B/50; ISO 306
 118 °C244 °FRate B/120; ISO 306
 
Optical PropertiesMetricEnglishComments
Yellow Index 6.0 %6.0 %ASTM D1925

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10073 / 243540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.