MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Pyrotek Ceramite® BCA/BCA-B Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® BCR and BCA Series are castable refractory materials based on bauxite and silicon carbide. Cast products from these refractories are widely used in the aluminium, ferroalloys, mining, cement and steel industries. The BCR aggregates have a maximum grain size of approximately 5 millimetres (0.20 inches). The BCA aggregates have a maximum grain size of approximately4 millimetres (0.16 inches). Different aggregates in each formulation determine the properties for each product. These refractory properties include good strength, good wear resistance, low thermal conductivity, good abrasion resistance and the ability to withstand thermal shock. The BCR series has a maximum service temperature of 1000°C (1832°F), and the BCA series has a maximum service temperature of 1500°C (2732°F).

Benefits:

  • Good strength
  • Good wear resistance
  • Low thermal conductivity
  • Thermal shock resistant

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.90 g/cc
Grain Size <= 4000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00700 GPa
@Temperature 20.0 °C
Cold
 0.0150 GPa
@Temperature 600 °C
Cold
 0.0170 GPa
@Temperature 850 °C
Cold
 0.0180 GPa
@Temperature 1000 °C
Cold
 0.0240 GPa
@Temperature 1000 °C
Hot
Compressive Strength 51.0 MPa
@Temperature 20.0 °C
Cold
 143 MPa
@Temperature 600 °C
Cold
 164 MPa
@Temperature 850 °C
Cold
 199 MPa
@Temperature 1000 °C
Cold
Abrasion 1.4
@Temperature 600 °C
[cm^3]
 1.9
@Temperature 20.0 °C
[cm^3]
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 4.40 W/m-K
@Temperature 900 °C
 4.90 W/m-K
@Temperature 600 °C
 6.10 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air 1000 °C
Shrinkage -0.500 %
@Temperature 20.0 - 850 °C
 
Descriptive Properties
Permanent Linear Change-0.3%20-850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CPYRO505 / 199527

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.