MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.

Applications: Grocery sacks, shopping bags, liners notion and millinery bags.

Advantages: High extrusion rate with high film strength and rigidity, excellent drawdown for high quality thin film.

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.950 g/cc0.0343 lb/in³ASTM D1505
Thickness 17.0 microns0.669 milextruded at 4:1 BUR
Base Resin Melt Index 0.10 g/10 min0.10 g/10 minI2; ASTM D1238
 11 g/10 min11 g/10 minI21; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ASTM D882
Film Elongation at Break, TD 700 %700 %ASTM D882
Elmendorf Tear Strength, MD 0.400 g/micron10.2 g/milASTM D1922
Elmendorf Tear Strength, TD 3.00 g/micron76.2 g/milASTM D1922
Dart Drop 8.00 g/micron203 g/milASTM D1709
Film Tensile Strength at Break, MD 58.8 MPa8530 psiASTM D882
Film Tensile Strength at Break, TD 44.1 MPa6400 psiASTM D882
1% Secant Modulus, MD 1176.8 MPa170680 psiASTM D882
1% Secant Modulus, TD 1280 MPa185000 psiASTM D882
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 240 °C356 - 464 °F
Blow-up Ratio (BUR) 4.04.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
Alclad Aluminum 7075-T6, T651
Akro-Plastic Akromid® B3 1 L natural (4685) PA6 + PP, Dry, 30% Glass Filled

PTITAN44 / 70410

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.