MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro ULTRACEL® U3000 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Ultracel U3000 (U-3000) is a stable 10% SAN-solids dispersion in a high molecular weight reactive base polyol.

Properties / Applications: Ultracel U3000 (U-3000) is a stable 10% SAN solids dispersion in a high molecular weight reactive base polyol. It is used in the production of high support (HS) and high resilience (HR) flexible slabstock foam having excellent comfort and durability and good physical properties. The primary applications are in premium quality furniture and mattresses. Ultracel U3000 produces very stable, yet shrink resistant, HS-HR foam that is easy to crush. It can be processed over a wide range of water levels and isocyanate indexes and in combination with varying amounts of high solids polymer polyols such as Arcol® HS-100 or Hyperlite® E-850. This provides unsurpassed flexibility for producing a wide range of foam grades of excellent quality. It can also be formulated with various foam modifiers, FRs, softening agents, and other additives to yield foams with unique performance features for specialized applications (supersoft cushion wrap, latex replacement, CMHR, etc.). As with any product, use of Ultracel U3000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
Viscosity 1700 cP1700 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 220 °C428 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %
 
Descriptive Properties
AppearanceWhite viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
LyondellBasell Petrothene® LR686001 High Density Polyethylene
Lanxess Uniplex 260 Plastic Additive
Ipiranga Petrochem GF 4960 HDPE
Evonik TEGOMER® DA 100 N Dispersant

PCOVEST1001 / 202784

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.