MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This material also has a high heat deflection temperature, good creep resistance, tensile and flexural strength and high rigidity. It has outstanding electrical properties, even at high frequencies and temperatures and is rated UL94 V-0 at 1/32" or 0.031"(0.8 mm) in all colors. Humidity resistance is another key feature. Mindel B-322 retains a high level of mechanical and electrical properties even at elevated temperatures, which can make it a suitable replacement for high performance thermosets. - Black: Mindel B-322 BK 1045

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccASTM D792
Water Absorption 0.14 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cmASTM D955
Melt Flow 4.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength 103 MPaASTM D638
Elongation at Break 2.5 %ASTM D638
Flexural Strength 159 MPaASTM D790
Flexural Modulus 6890 MPaASTM D790
Izod Impact, Notched 53.4 J/mASTM D256
Tensile Impact Strength 84.1 kJ/m²ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 1000 Hz
ASTM D150
 3.7
@Frequency 1e+6 Hz
ASTM D150
 3.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 1.60 mm
Method B (Step-by-Step); ASTM D149
 20.0 kV/mm
@Thickness 3.18 mm
Method A (Short-Time); ASTM D149
 29.0 kV/mm
@Thickness 0.800 mm
Method B (Step-by-Step); ASTM D149
 30.0 kV/mm
@Thickness 0.800 mm
Method A (Short-Time); ASTM D149
Dissipation Factor 0.0020
@Frequency 60 Hz
ASTM D150
 0.0030
@Frequency 1000 Hz
ASTM D150
 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 27.0 µm/m-°CASTM D696
Thermal Conductivity 0.220 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 160 °CUnannealed; ASTM D648
UL RTI, Electrical 160 °CUL 746
UL RTI, Mechanical with Impact 160 °CUL 746
UL RTI, Mechanical without Impact 160 °CUL 746
Flammability, UL94 V-0
@Thickness 0.790 mm
UL 94
Oxygen Index 35 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 271 - 316 °C
Mold Temperature 65.6 - 98.9 °C
Drying Temperature 135 - 163 °C
@Time 10800 - 14400 sec
Moisture Content 0.020 %
 
Descriptive Properties
AdditiveFlame Retardant
AppearanceColors Available
 Natural Color
AvailabilityAsia Pacific
 Europe
 North America
 South America
FeaturesFlame Retardant
 Good Chemical Resistance
 Good Dimensional Stability
 High Rigidity
 Warp Resistant
FormsPellets
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant
Suggested Max Regrind, %25
UsesAppliance Components
 Appliances
 Business Equipment
 Electrical Housing
 Electrical Parts
 Electrical/Electronic Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
Syensqo (Solvay Specialty Polymers) Mindel® B-430 Polysulfone, Modified (PSU, Modified)
RTP Company RTP 2000 B-430 Polysulfone Alloy Glass Fiber - Flame Retardant
Syensqo (Solvay Specialty Polymers) Mindel® S-1000 Modified Polysulfone

PSOL8Y921 / 107705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.