MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell CirculenRecover C14 LD3020K LDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: CirculenRenew C14 LD3020 K is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 LD3020 K is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 LD3020 K is a non-additivated, low density polyethylene. It is characterized by a good processability. LyondellBasell customers report that films made from CirculenRenew C14 LD3020 K exhibit a glossy surface finish. CirculenRenew C14 LD3020 K provides the option to produce films with very good optical properties. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications.

Status: Commercial - Active

Availability: Europe

Application: Food Packaging Film; Lamination Film; Shrink Film; Surface Protection Film

Market: Flexible Packaging

Processing Method: Blown Film; Cast Film; Injection Molding

Attribute: Good Heat Seal; Good Processability; Superior Optical Properties

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccISO 1183-1
Melt Flow 4.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 13.0 MPaISO 527-1, -2
Film Elongation at Break, MD 350 %ISO 527-1, -3
Film Elongation at Break, TD 600 %ISO 527-1, -3
Tensile Modulus 300 MPaISO 527-1, -2
Coefficient of Friction >= 0.800ISO 8295
Dart Drop Test 90.0 gF50; ASTM D1709
Film Tensile Strength at Break, MD 20.0 MPaISO 527-1, -3
Film Tensile Strength at Break, TD 17.0 MPaISO 527-1, -3
 
Thermal PropertiesOriginal ValueComments
Melting Point 114 °CPeak; ISO 11357-3
Vicat Softening Point 97.0 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze <= 7.00 %
@Thickness 0.0500 mm
ASTM D1003
Gloss >= 80.0 %20°; ASTM D2457
 >= 115 %60°; ASTM D2457
 
Descriptive Properties
Failure Energy3.5 J/mmDIN 53373

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9084 / 324019

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.