MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC SABIC® HDPE F01552 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: SABIC® HDPE F01552 is a medium molecular weight High Density Polyethylene specifically designed for blown film extrusion. It has a broad molecular weight with excellent extrudability, high film strength and draw down characteristics. The material contains anti oxidant.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D1505
Melt Flow  0.15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 16 g/10 min
@Load 21.6 kg,
Temperature 190 °C
16 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 31.0 MPa4500 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
Film Tensile Strength at Yield, TD 30.0 MPa4350 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
Film Elongation at Break, MD 400 %400 %Properties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
Film Elongation at Break, TD 610 %610 %Properties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
Elmendorf Tear Strength MD 4.0 g4.0 gASTM D1922
Elmendorf Tear Strength TD 40 g40 gASTM D1922
Dart Drop Test 180 g0.397 lbASTM D1709
Film Tensile Strength at Break, MD 55.0 MPa7980 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
Film Tensile Strength at Break, TD 49.0 MPa7110 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
1% Secant Modulus, MD 1400 MPa203000 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
1% Secant Modulus, TD 1700 MPa247000 psiProperties are based on 15 µm film produced at a BUR of 4 using 100% F01552.; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 125 °C257 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10905 / 244372

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.