Moplen HP554M is a polypropylene homopolymer suitable for extrusion applications. Moplen HP554M is formulated with an anti-gasfading stabilization package and is used for the production of fine denier staple fibers. Typical application is nonwovens. Availability: Africa-Middle East; Europe Application: Filament Yarn Market: Textile Processing Method: Continuous Filament/Spinning; Staple Fiber Attribute: Homopolymer Information provided by LyondellBasell. |