MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® MP-2111 L2 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccASTM D792
Linear Mold Shrinkage 0.020 cm/cm0.020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838ASTM D2240
Tensile Strength at Break 4.14 MPa600 psiASTM D412
Tensile Stress at Strain 2.07 MPa
@Strain 300 %
300 psi
@Strain 300 %
ASTM D412
Elongation at Break 650 %650 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 232 °C360 - 450 °F
Middle Barrel Temperature 188 - 238 °C370 - 460 °F
Front Barrel Temperature 193 - 243 °C380 - 470 °F
Nozzle Temperature 199 - 249 °C390 - 480 °F
Zone 1 182 - 232 °C360 - 450 °F
Zone 2 188 - 238 °C370 - 460 °F
Zone 3 193 - 243 °C380 - 470 °F
Zone 5 199 - 249 °C390 - 480 °F
Die Temperature 199 - 249 °C390 - 480 °F
Melt Temperature 199 - 249 °C390 - 480 °FProcessing Temperature
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
Acid and Base Resistance8PDL Resistance Rating
Alcohol Resistance6PDL Resistance Rating
AppearanceClear/Transparent
Sebum Oil Swell (%)12at 50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNP733 / 129835

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.