Semi crystalline ethylene-propylene rubber with medium Mooney viscosity. The low level of unsaturation ensures excellent heat ageing performance, especially when peroxide cured, the polymer structure ensures a good balance between processing, physical properties and low temperature performance.Information provided by Lanxess. |