MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Spartech PE4130 Reinforced High Density Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer an excellent balance of stiffness, impact resistance and dimensional stability. Typical applications for blow molding grades include automotive seat cores, heating ducts, and recreational products such as ice chests.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/cc
@Temperature 22.8 °C
ASTM D792
Filler Content 30 %Talc
Linear Mold Shrinkage 0.013 in/in0.125inch wall
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4700 psiASTM D638
Elongation at Break 30 %ASTM D638
Elongation at Yield 8.0 %ASTM D638
Flexural Strength 6800 psiMax Load; ASTM D790
Flexural Modulus 235000 psisecant; ASTM D790
 310000 psitangent; ASTM D790
Izod Impact, Notched 3.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 6.00 ft-lb
@Temperature -5.56 °C
ASTM D5420
 >= 25.0 ft-lb
@Temperature 22.8 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2652 Polycarbonate
RTP Company PermaStat® 700 High Density Polyethylene (HDPE); ESD Protection - Permanently Anti-static
ExxonMobil HD 7845.30 High Density Polyethylene Resin
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding

PSPAR136 / 78758

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.