MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Radel® WM PPSU
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Radel® WM Polyphenylsulfone (PPSU) is a transparent and rigid high-temperature engineering thermoplastic and belongs to the sulfone family of polymers. PPSU is the highest performing sulfone polymer. It is known for its extreme toughness, high flexural and tensile strength, excellent hydrolytic stability and good resistance to chemicals and heat. It is highly resistant to aqueous mineral acids, bases, and oxidizing agents and most solvents. It excels in high heat and humidity environments and provides operating temperatures around 200°C (392°F). Westlake’s Radel® WM stock shapes are made exclusively from Solvay, Radel® PPSU. Its regulatory compliance profile and lot-traceability make it ideal for use in medical and life science applications. Sterilization methods include EtO gas, radiation, steam autoclaving, dry heat, and cold sterilization. PPSU is intrinsically flame retardant, and offers high impact strength and good chemical resistance. PPSU is often an excellent choice for components that are exposed to high temperatures and corrosive media because of its exceptional chemical resistance. Examples include pipe fittings, battery containers, medical device parts, and sterilizable products for healthcare applications. Polyphenylsulfone is also used in the automotive and aerospace industries for applications where superior thermal and mechanical properties relative to other engineering grade resins are required.

Industry: Life Sciences

Colors Available: Black, Orange, Purple, Natural, Grey, Light Grey, Brown, Yellow, Red, Dark Grey, Bone, Green

Attributes: Dimensional Stability; Biocompatibility; Impact Resistance; Chemical Resistance; Heat Resistant

Shapes: Extruded Slab; Compression Sheet; Extruded Sheet; Extruded Film; Extruded Rod

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Water Absorption 0.37 %
@Time 86400 sec
0.37 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.6 MPa10100 psiASTM D638
Elongation at Break 60 - 120 %60 - 120 %ASTM D638
Elongation at Yield 7.2 %7.2 %ASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 89.6 MPa
@Strain 5.0 %
13000 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 6.94 J/cm13.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C404 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEST919 / 243164

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.