MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Plansee MoNa Molybdenum-Sodium (Mo-2.6%Na) Sputtering Target
Categories: Metal; Nonferrous Metal; Molybdenum Alloy

Material Notes: High purity. Fine microstructure: The sodium compound resides between the molybdenum grains. Because it is produced by powder metallurgical methods, the sodium particles are particularly fine and evenly distributed. The electrical conductivity of a MoNa target is slightly lower than that of a pure molybdenum target, but still perfectly sufficient to perform sputtering in DC mode. Sodium levels of 1.3% and 2.6% (by weight) are available; property data reported is for 2.6% Na.

Used in CIGS solar cells.

Information provided by PLANSEE.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density >= 7.40 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000204 ohm-cm
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0030 %<30 ppm by weight
Cadmium, Cd 0.00050 %<5 ppm by weight
Carbon, C 0.020 %<200 ppm by weight
Chromium, Cr 0.00050 %<5 ppm by weight
Cobalt, Co 0.0010 %<10 ppm by weight
Iron, Fe 0.0030 %<30 ppm by weight
Lead, Pb 0.00050 %<5 ppm by weight
Manganese, Mn 0.00020 %<2 ppm by weight
Mercury, Hg 0.00010 %<1 ppm by weight
Molybdenum, Mo 97.4 %
Nickel, Ni 0.0010 %<10 ppm by weight
Oxygen, O 4.0 %<40000 ppm by weight
Sodium, Na 2.6 %
Tungsten, W 0.10 %<1000 ppm by weight
 
Descriptive Properties
Purity>99,97%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPLAM976 / 249330

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.