MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ISONATE™ 181 MDI Prepolymer
Categories: Fluid

Material Notes: ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscosity, super-cooled liquid provides more rapid compatibility between isocyanates and polyols, which increases the effectiveness of catalysts present and usually results in a more easily controlled polymer reaction.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.221 g/cc
Viscosity 770 cP
Viscosity Measurement 5.0 - 10[cps/mo.] Viscosity growth
Vapor Pressure <= 1.30e-8 bar
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.010HCl content, %
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 86.0 cal/g
CTE, linear 737 µin/in-°F
@Temperature 20.0 °C
Specific Heat Capacity 1.80 J/g-°C
Thermal Conductivity 0.000300 cal cm/sec-cm²-°C
Boiling Point 314 °C
Decomposition Temperature 230 °C
Flash Point >= 351 °FASTM D93 Closed Cup
 
Descriptive Properties
NCO Content %23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ISONATE™ 143L Modified MDI
Dow ISONATE™ 50 O,P` Pure MDI
Dow ISONATE™ 240 MDI Prepolymer
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
Celanese 50000767 91-93% Paraformaldehyde

PDOW1385 / 30603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.