MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK 8387BS Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Product Benefits:

  • Non-conductive
  • Black pigmentation for blocking stray light
  • 30µm polymer spacers for bondline thickness control
Cure: Heat cure

Application: Die attach

LOCTITE ABLESTIK 8387BS single component adhesive is designed for high throughput bonding applications. It contains spacers for improved bondline control.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 14250 cPUncured, CP51, Speed 5 rpm
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 75.0 MPa
@Temperature 250 °C
Cured, DMTA
 87.0 MPa
@Temperature 200 °C
Cured, DMTA
 118 MPa
@Temperature 150 °C
Cured, DMTA
 790 MPa
@Temperature 100 °C
Cured, DMTA
 1919 MPa
@Temperature 25.0 °C
Cured, DMTA
 3529 MPa
@Temperature -65.0 °C
Cured, DMTA
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 122 °CCured, TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 100 °C
 1.50 min
@Temperature 90.0 °C
Alternate Cure Schedule
Working Life 48.0 hour
Shelf Life 12.0 MonthUncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)<10Cured, Sodium (Na+)
 <10Cured, Potassium (K+)
 <50Cured, Chloride (Cl-)
Shear Strength>14 kg-fDie, 3 X 3 mm Si die, Ag/Cu Leadframe
Thixotropic Index>4.5Uncured, 0.5/5 rpm
Weight Loss (%)0.59Cured Paste, Cured, @ 300ºC
 0.74Wet Paste, Cured, @ 300ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5032 / 255243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.