Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Type:
Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.
Feature:
Film resin, Fuel resistant, Blow molding grade resin.
Information Provided by The Lubrizol Corporation
Key Words:
TPU
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.22
g/cc
1.22
g/cc
ASTM D792
Linear Mold Shrinkage
0.0050
-
0.0090
cm/cm
0.0050
-
0.0090
in/in
Transverse direction; ASTM D955
Linear Mold Shrinkage, Flow
0.0060
-
0.0090
cm/cm
0.0060
-
0.0090
in/in
ASTM D955
Melt Flow
13
g/10 min
@Load 8.70 kg,
Temperature 190 °C
13
g/10 min
@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
94
94
ASTM D2240
Tensile Strength, Ultimate
38.9
MPa
5640
psi
ASTM D412
Elongation at Break
450 %
450 %
ASTM D412
50% Modulus
8.30
MPa
@Strain 50 %
8.30
MPa
@Strain 50 %
ASTM D412
100% Modulus
9.70
MPa
@Strain 100 %
1410
psi
@Strain 100 %
ASTM D412
300% Modulus
21.4
MPa
@Strain 300 %
3100
psi
@Strain 300 %
ASTM D412
Flexural Modulus
0.0896
GPa
13.0
ksi
ASTM D790
Tear Strength
105
kN/m
599
pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles
4.0
4.0
H-22 (coarser); ASTM D1044
Compression Set
30 %
@Temperature 25.0 °C,
Time 79200 sec
30 %
@Temperature 77.0 °F,
Time 22.0 hour
Method B; ASTM D395
80 %
@Temperature 70.0 °C,
Time 79200 sec
80 %
@Temperature 158 °F,
Time 22.0 hour
Method B; ASTM D395
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
153
µm/m-°C
85.0
µin/in-°F
ASTM D696
Vicat Softening Point
80.6
°C
@Load 0.999 kg
177
°F
@Load 2.20 lb
120°C/hr, 9.8N; ASTM D1525
Glass Transition Temp, Tg
-15.0
°C
5.00
°F
DSC
Processing Properties
Metric
English
Comments
Melt Temperature
182
-
199
°C
360
-
390
°F
Extrusion
Mold Temperature
16.0
-
60.0
°C
60.8
-
140
°F
Drying Temperature
88.0
-
104
°C
190
-
219
°F
Air dew point <-40°C
Descriptive Properties
Elongation Set After Break (%)
60
ASTM D412
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PNOVEON550 / 121441
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.