MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kraton® D1101 B (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identified:
Kraton D1101 BT - supplied as a dusted porous pellet
Kraton D1101 BTM - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America and South America

Uses: Kraton D1101 B is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 2781
Bulk Density 0.400 g/ccASTM D 1895 method B
Volatiles <= 0.30 %KM 04
Brookfield Viscosity 3000 - 5000 cPMeasured on 25% mass solution in toluene at 25°C; KM 06
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash 0.30 - 0.60 %BT; ISO 247
 <= 5.0 %BTM; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 10.0 sec
Measure on compression molded slabs; ISO 868
Tensile Strength 33.0 MPameasured on films cast from a solution in toluene; ISO 37
Elongation at Break 880 %Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00290 GPa
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentAntioxidants>0.1%, KM 08
 Polystyrene30-32%, KM 03
 Total Extractables<1.0%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® G1702 + PPE blend (20/80)
Kraton® D1101 E (SBS) Liner Block Copolymer
Kraton® D1102 B (SBS) Liner Block Copolymer

PKRA9804 / 132703

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.