Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min. Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transparency. It is suitable for the injection molding of transparent packaging. Information provided by Total Petrochemicals. |