MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ECO Brass, Copper Alloy, UNS C69300, M30 Temper, Plate
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Hot Formed; Good Suitability – Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Poor Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Forming and Bending; Machining; Shearing

Typical uses: Fluid Connectors; Sensor Bodies; Thermostat Parts; Automatic Screw Machine Parts; Bolts; Condenser Tube Plate; Nuts; Pneumatic Fittings; Pump Parts; Screw Machine Products; Valve Bodies for Water; Valve Stems; Marine Products; Propeller Shafts; Faucet Stems; Faucets; Plumbing Fittings; Water Meter Cases

Applicable Specifications: Die Forging – ASTM B283/B283M; Rod – ASTM B371/B371M; Rod, Bar & Shapes – Forgings ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 81
@Thickness 25.4 mm
81
@Thickness 1.00 in
Tensile Strength 517 MPa
@Thickness 25.4 mm
75000 psi
@Thickness 1.00 in
Tensile Strength, Yield  241 MPa
@Thickness 25.4 mm
35000 psi
@Thickness 1.00 in
0.2% Offset
 248 MPa
@Thickness 25.4 mm
36000 psi
@Thickness 1.00 in
0.5% Ext
Elongation at Break >= 15 %
@Thickness 25.4 mm
>= 15 %
@Thickness 1.00 in
Tensile Modulus 105 GPa15200 ksi
Machinability 85 %85 %
Forgeability 95 %95 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm8% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  18.5 µm/m-°C
@Temperature 20.0 - 100 °C
10.3 µin/in-°F
@Temperature 68.0 - 212 °F
 18.5 µm/m-°C
@Temperature 20.0 - 200 °C
10.3 µin/in-°F
@Temperature 68.0 - 392 °F
 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 3.14 W/m-K21.8 BTU-in/hr-ft²-°F
Melting Point 855.0 - 880.0 °C1571 - 1616 °F
Solidus 855.0 °C1571 °F
Liquidus 880.0 °C1616 °F
Annealing Point 500 - 600.0 °C932 - 1112 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 73 - 77 %73 - 77 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni <= 0.10 %<= 0.10 %
Phosphorus, P 0.040 - 0.15 %0.040 - 0.15 %
Silicon, Si 2.7 - 3.4 %2.7 - 3.4 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn 19 - 24.3 %19 - 24.3 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC69300x3 / 292374

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.