MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco AREMCOLOX™ 502-1600 (99%) Machinable Boron Nitride 99%
Categories: Ceramic; Machinable Ceramic; Nitride

Material Notes: Hot-pressed boron nitride provides high thermal conductivity, electrical insulation, and low coefficient of thermal expansion. Grades are non-reactive with molten salts, aluminum and other metals. Easily machined and available in plates from ¼” to 1” thick; rods from ¼” to 3” diameter by 12” long, and bars from ¼” × ¼” to 2” × 2”.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 19
Flexural Strength 12300 psi
Compressive Strength 5080 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Dielectric Strength 865 V/mil
Dissipation Factor <= 0.00020
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.200 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 50.0 W/m-K
Maximum Service Temperature, Air 900 °COxidizing
Maximum Service Temperature, Inert 2200 °C
 3270 °FVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1550 (Med. Density) Machinable Zirconium Phosphate
Corning Macor® Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94%
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride
Misumi Machinable SiO2-MgO Ceramic

CAREM10 / 551

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.