MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller Cyberbond SM 40 Adhesive
Categories: Polymer; Adhesive

Material Notes: Profile: Threadlocking and sealing; medium strength, medium viscosity. Anaerobic adhesive for hydraulic and pneumatic applications; fine thread.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Viscosity 60 - 80 cP
@Shear Rate 160 1/s
cone-plate
 1000 - 2000 cP
@Shear Rate 0.500 1/s
cone-plate
Storage Temperature 8.00 - 21.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 6.00 - 12.0 MPa
@Time 86400 sec
Steel pin/collar specimen
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull Cure
 20.0 - 45.0 secSet time, M10 brass bolt/nut
Shelf Life 12.0 Month
 
Descriptive Properties
Adhesive strength6-12 NmStainless steel V2A
 8-14 NmGalvanized steel
 8-14 NmBrass
 8-14 NmSteel
Base compoundDimethacrylate
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL050 / 316841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.