MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil 1 Synthetic ATF
Categories: Fluid; Lubricant

Material Notes: Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.

Mobil 1 Synthetic ATF is a multi-vehicle formula recommended for use in modern high performance automobiles, SUVs, SUTs, vans and other light trucks requiring Dexron III , Ford Mercon and Mercon V performance levels; Also recommended by ExxonMobil for Chrysler automatic transmissions; Surpasses the off-highway power transmission requirements of Allison C-4; Suitable for Caterpillar TO-2 applications; Recommended for use in any power steering unit where a Dexron or Mercon fluid is recommended

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 5190 cP
@Temperature -40.0 °C
ASTM D5293
Viscosity Measurement 199Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 34 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.6 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -54.0 °CASTM D97
Flash Point 236 °CASTM D92
 
Descriptive Properties
Colorred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON047 / 75472

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.