MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. Thermoformed parts have greater polystyrene acceptance with equivalent processability, very good clarity, excellent toughness, and good stiffness.

Applications: Major applications include thermoformed blister packs, cups and lids, and portion packages.

Processing Recommendations:
Melt Temperature: 216°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.

Specification Data: When combined with at least 17% food grade polystyrene to produce articles for food contact, KK38 complies with FDA Regulation 21 CFR 177.1640. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL94HB.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58ASTM D2240
Tensile Strength, Yield 13.1 MPaType 1 @ 2 in/min; ASTM D638
Elongation at Break 180 %Type 1 @ 2 in/min; ASTM D638
Flexural Yield Strength 18.6 MPaASTM D790
Flexural Modulus 1.055 GPaASTM D790
Izod Impact, Notched NB
@Thickness 3.17 mm
ASTM D256
Impact Test 28.4 J
@Thickness 3.17 mm
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CASTM D648
Vicat Softening Point 76.0 °CASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 89 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 216 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade

PCHEVK40 / 20281

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.