MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Vestoran® RD 3530 SBR Rubber/Plastic Composite  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement  >= 2.8
@Temperature 180 °C
>= 2.8
@Temperature 356 °F
Rheometer, t10
 >= 5.9
@Temperature 180 °C
>= 5.9
@Temperature 356 °F
Rheometer, t90
Mooney Viscosity 85
@Temperature 100 °C
85
@Temperature 212 °F
ML (1 + 4)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868
 46
@Temperature 75.0 °C
46
@Temperature 167 °F
Tensile Strength at Break 18.6 MPa2700 psi
Elongation at Break 378 %378 %
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
200% Modulus 8.50 MPa
@Strain 200 %
1230 psi
@Strain 200 %
300% Modulus 15.5 MPa
@Strain 300 %
2250 psi
@Strain 300 %
Rebound 46 %46 %23°C
 
Descriptive Properties
Formulation as Tested1Stearic Acid
 1Vulkacit®NZ(TBBS)
 1.75Sulfur
 100SBR 1500
 3ZnO
 5Paraffin Oil
 50Carbon Black N 550

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mallard Creek Polymers Rovene® 4813 Non-Carboxylated Styrene-Butadiene Emulsion
Synthos SPRINTAN™ SLR 3402-SCHKOPAU Solution-Styrene Butadiene Rubber (S-SBR)
Rubatex R8702 SBR Rubber Foam Sheet

PHUMA81 / 47595

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.