MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipchem Sahara C 700HTP Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: SAHARA C 700HTP is a nucleated impact copolymer used for injection molding and compounding applications. It exhibits good impact to stiffness balance combined with high fluidity with very good organoleptic properties. SAHARA C 700HTP is typically used in opaque containers, housewares, toys and in thin wall containers for food packaging e.g. Margarine tubs, Yoghurt pots and compounding applications.

Product Characteristics:
Commercial Status: Experimental grade.
Processing Method: Injection Molding
Typical applications: Thin wall containers; housewares.

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO1183-1
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
70 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiISO 527-1, -2
Elongation at Break 4.4 %4.4 %ISO 527-1, -2
Elongation at Yield 3.4 %3.4 %ISO 527-1, -2
Tensile Modulus 1.57 GPa228 ksiISO 527-1, -2
Flexural Modulus 1.61 GPa234 ksiISO 178
Izod Impact, Notched 0.0380 J/cm0.0712 ft-lb/inISO 180
Charpy Impact, Notched  0.300 J/cm²
@Temperature -20.0 °C
1.43 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise; ISO 179
 0.340 J/cm²
@Temperature 0.000 °C
1.62 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise; ISO 179
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °Funannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °Funannealed; ISO 75B-1, -2
Vicat Softening Point 70.0 °C158 °FB50; ISO 306
 147 °C297 °FA50; ISO 306
Shrinkage 1.0 - 2.5 %1.0 - 2.5 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 250 °C410 - 482 °FBarrel temperature range
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 15.0 - 40.0 °C59.0 - 104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPCH036 / 285349

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.