Introduction: This series of polyether polyols is designed according to the individual needs of customers. They are mostly 2 or 3 functionality with different molecular weight from 400 to 5000. Applications: Foam-opening agent for high resilience foams to improve the open ability of foam and reduce foam shrinkage Information provided by Shandong INOV Polyurethane Co., Ltd. |