MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Raschig Group RALUPOL® 2100 UP Polyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection and compression molding

Primary application: Safety cut outs, Contactors, Switches

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 - 1.85 g/ccISO 1183
Apparent Bulk Density 0.750 - 1.00 g/ccISO 60
Water Absorption <= 1.2 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cmInjection; ISO 2577
 0.0080 - 0.011 cm/cmCompression; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.0 - 40.0 MPaCompression; ISO 527
 40.0 - 50.0 MPaInjection; ISO 527
Modulus of Elasticity 4.00 - 6.00 GPaCompression; ISO 527
 5.00 - 8.00 GPaInjection; ISO 527
Flexural Strength 50.0 - 80.0 MPaCompression; ISO 178
 80.0 - 120 MPaInjection; ISO 178
Flexural Modulus 6.00 - 9.00 GPaCompression; ISO 178
 7.00 - 10.0 GPaInjection; ISO 178
Compressive Strength 150 - 200 MPaISO 604
Charpy Impact Unnotched 5.00 - 8.00 kJ/m²Compression; ISO 179/1eU
 6.00 - 10.0 kJ/m²Injection; ISO 179/1eU
Charpy Impact, Notched 1.00 - 2.00 kJ/m²Compression; ISO 179/1eA
 1.50 - 2.50 kJ/m²Injection; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 - 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+11 - 1.00e+12 ohmIEC 60093
Dielectric Constant 4.0 - 6.0
@Frequency 1e+6 Hz
IEC 60250
 5.0 - 7.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 - 30.0 kV/mmIEC 60243-1
Dissipation Factor 0.030 - 0.050
@Frequency 1e+6 Hz
IEC 60250
 0.60 - 0.80
@Frequency 100 Hz
IEC 60250
Arc Resistance 180 - 240 secASTM D495
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 24.0 - 45.0 µm/m-°C
@Temperature 50.0 - 100 °C
ISO 11359-2
Thermal Conductivity 0.900 - 1.00 W/m-KASTM E1461
Maximum Service Temperature, Air 190 °C
@Time <=180000 sec
IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) >= 180 °CISO 75-A
Deflection Temperature at 8.0 MPa 80.0 - 120 °CISO 75-C
Flammability, UL94 V-0
@Thickness 3.00 mm
Shrinkage 0.20 - 0.40 %
@Temperature 110 °C,
Time 605000 sec
Post shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
 
Descriptive Properties
Glow wire flammability test960/1IEC 60695 2-12
Glow wire ignitability test850/1IEC 60695 2-13
Water Absorption<75 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 1901 Mineral Filled Alkyd
Plenco 08133 Polyester BMC, Compression Molded
Overview of materials for Silicone Rubber
Envalior Durethan® BKV 30 HTS 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned

PRASCI11 / 179148

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.