MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

1-Propanol (Propyl alcohol), C3H8O
Categories: Fluid; Solvent

Key Words: C3H8O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.804 g/cc
@Temperature 20.0 °C
0.0290 lb/in³
@Temperature 68.0 °F
Viscosity 2.204 cP
@Temperature 20.0 °C
2.204 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 60.096 g/mol60.096 g/mol
Vapor Pressure 0.01941 bar
@Temperature 20.0 °C
14.56 torr
@Temperature 68.0 °F
Surface Tension 23.45 dynes/cm
@Temperature 20.0 °C
23.45 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 51.7 bar38800 torr
Critical Temperature 264 °C507 °F
Critical Density 0.274 g/cc0.00990 lb/in³
Critical Molar Volume 219 cm³/mol13.4 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 20.45
@Temperature 20.0 °C
20.45
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 694.8 J/g298.9 BTU/lb
Specific Heat Capacity 2.394 J/g-°C0.5722 BTU/lb-°F
 1.434 J/g-°C
@Temperature 25.0 °C
0.3427 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1553 W/m-K
@Temperature 20.0 °C
1.078 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -126.3 °C-195.3 °F
Boiling Point 97.3 °C207 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.386
@Wavelength 589.3 nm
1.386
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter17.5439
Antoine's Vapor Pressure B Parameter3166.38
Antoine's Vapor Pressure C Parameter-80.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)71-23-8
Chemical FormulaC3H8O
Critical Compressibility (Zc)0.253
Dipole moment (p/C.m)5.671E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A951.04
Dynamic Viscosity Parameter B327.83
Henry's Law Constant (atm m3/mol)6.85E-06
Molar Heat Capacity (298K)86.199 J/mol-K
Molar Heat Capacity of Vapor a Parameter2.4686
Molar Heat Capacity of Vapor b Parameter0.3323
Molar Heat Capacity of Vapor c Parameter-0.0001854
Molar Heat Capacity of Vapor d Parameter4.923E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1274
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper (II) Chloride, CuCl2
Ethanolamine, C2H7NO

VORGS299 / 99656

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.