MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott BG18 Band Pass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.

Key Words: DIN BP 480/250,DIN KP 605
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.68 g/cc0.0968 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 22
Alkali Class, AR 22
Stain Resistance Class, FR 0.00.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.40 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.11 µin/in-°F
@Temperature -22.0 - 158 °F
 8.80 µm/m-°C
@Temperature 20.0 - 300 °C
4.89 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 459 °C858 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.54
@Wavelength 587.6 nm
1.54
@Wavelength 587.6 nm
He
 1.55
@Wavelength 404.7 nm
1.55
@Wavelength 404.7 nm
Hg
Transmission, Visible  <= 1.0 %
@Wavelength 660 - 700 nm
<= 1.0 %
@Wavelength 660 - 700 nm
 83 %
@Wavelength 500 - 530 nm
83 %
@Wavelength 500 - 530 nm
Internal transmittance of 92% from 510-520 nm
IR Transmittance 72 %
@Wavelength 2400 nm
72 %
@Wavelength 2400 nm
Internal transmittance of 79% at 2400 nm.
UV Transmittance  <= 0.30 %
@Wavelength 200 - 320 nm
<= 0.30 %
@Wavelength 200 - 320 nm
 59 %
@Wavelength 390 nm
59 %
@Wavelength 390 nm
Internal transmittance of 64% at 390 nm
Reflection Coefficient, Visible (0-1) 0.91
@Wavelength 587.6 nm
0.91
@Wavelength 587.6 nm
Reflection Factor P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott RG630 Long Pass Filter
Schott KG2 Short Pass Filter
Schott BG3 Band Pass Filter
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 12.7 - 25.4 mm.

CSGT05 / 1994

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.