MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

TriSteel

TriStar TriSteel AT Metal Backed PTFE Bearing System
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, lift and tilt on medium speed and load applications. Liner thickness allows for secondary machining to accommodate misalignment or minor ID tolerance corrections.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Yield 51.7 MPa7500 psi
Elongation at Break 12 %12 %
Flexural Strength 103 MPa15000 psi
Flexural Modulus 1.03 GPa150 ksi
Compressive Yield Strength 117 MPa
@Strain 2 %
17000 psi
@Strain 2 %
Compressive Strength 172 MPa25000 psiMaximum Static Bearing Load
Compressive Modulus 2.14 GPa310 ksi
K (wear) Factor 161 x 10-8 mm³/N-M80.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 1.26 MPa-m/sec36000 psi-ft/minUnlubricated. Max P = 25,000 psi and max V = 300 fpm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.4 µm/m-°C18.0 µin/in-°F
Maximum Service Temperature, Air 82.2 °C180 °FContinuous
 98.9 °C210 °FShort Term
Brittleness Temperature -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TriStar TriSteel AC Metal Backed PTFE Bearing System
TriStar TriSteel PE Metal Backed PTFE Bearing System
Phosphorous, P, Red
TriStar TriSteel PR Metal Backed PTFE Bearing System
TriStar TriSteel PT Metal Backed PTFE Bearing System

PTRIST991 / 176085

TriSteel

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.