MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® ASA 540/7 UV SV1281-08MCF ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Base Polymer: Acrylonitrile/Styrene/Acrylate/Copolymer

Color: metallic effect, similar to RAL 9006

Special Features: Low tendency to flow lines, UV stabilized

Market Segment: Electrical and Electronic, Building and Construction, Sport and Leisure

Application Area: Housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 100 MPaH358/30; ISO 2039-1
Tensile Strength 49.0 MPaISO 527
Tensile Strength, Yield 49.0 MPaISO 527
Elongation at Break 6.0 %ISO 527
Elongation at Yield 3.1 %ISO 527
Tensile Modulus 2700 MPaISO 527
Flexural Strength 77.0 MPaISO 178
 73.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2900 MPaISO 178
Charpy Impact Unnotched 15.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 20.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eU
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 3.50 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+12 ohmDIN EN 62631-3-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CISO 75-1/-2
Vicat Softening Point 102 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
Glow Wire Flammability Index 650 °C
@Thickness 1.00 mm
passed; DIN EN 60695
 650 °C
@Thickness 2.00 mm
passed; DIN EN 60695
 650 °C
@Thickness 3.00 mm
passed; DIN EN 60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °CInjection molding
Mold Temperature 40.0 - 80.0 °CInjection molding
Drying Temperature <= 80.0 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 <= 80.0 °C
@Time 10800 - 21600 sec
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitrile/Styrene/Acrylate/Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALBIS8445 / 242504

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.