MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot CABELEC® CA6397 TPU, Conductive Compound
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product highlights: CABELEC CA6397 conductive compound is suitable for use in injection molded thermoplastic polyurethane ester base (TPU). It is made with a carefully selected conductive carbon black that can enable excellent mechanical properties and superior abrasion resistance in end-use products.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Melt Flow 30 g/10 min
@Load 190 kg,
Temperature 21.6 °C
30 g/10 min
@Load 419 lb,
Temperature 70.9 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 96
@Time 15.0 sec
96
@Time 0.00417 hour
ISO 868
Hardness, Shore D 42
@Time 15.0 sec
42
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 23.0 MPa3340 psiISO 527
Elongation at Break 377 %377 %ISO 527
Flexural Modulus 0.0830 GPa12.0 ksiISO 178
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmIEC 61340-2-3
Surface Resistance <= 1000 ohm<= 1000 ohmIEC 61340-2-3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 32.0 °C89.6 °FISO 75/2
Vicat Softening Point 84.0 °C
@Load 1.02 kg
183 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 °C356 °Fbarrel
Nozzle Temperature 200 °C392 °F
Mold Temperature 60.0 °C140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT048 / 315783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.