MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UNS C84200, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: Pipe fittings, elbows, T's, couplings, bushings, locknuts, plugs, unions.

Classified under: Semi-red brasses and leaded semi-red brasses

As cast values below are for sand casting. Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.70 g/ccEstimated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60500 kg
Tensile Strength, Ultimate 193 MPaas cast
Tensile Strength, Yield 103 MPaas cast
Elongation at Break 27 %as cast
Tensile Modulus 14000 ksi
Machinability 80 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000105 ohm-cm16.4% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 41.8 BTU-in/hr-ft²-°F
Melting Point 1540 - 1820 °F
Solidus 1540 °F
Liquidus 1820 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 80 %
Lead, Pb 2.5 %
Tin, Sn 5.0 %
Zinc, Zn 12.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
UNS C80900, Copper Casting Alloy
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
UNS C80100, Copper Casting Alloy
Leaded Semi-Red Brass (Valve Metal), UNS C84400, Copper Casting Alloy
UNS C81300, Copper Casting Alloy

MC84200b1 / 11903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.