MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt ARMORCOTE® GPLY 8000-061 Neutral Armorcote Spray Gel Coat
Categories: Polymer; Thermoset

Material Notes: Neutral gel coat base to color match, Medium reactivity, accelerated, Light stabilized, Superior weather resistance.
Process: Airless or air atomized spray gun equipment, Gel coat delivery rate less than 2.5 pounds/minute with conventional air atomized equipment and less than 4 pounds/minutes with airless equipment.
Applications: Marine, transportation, Transportation, building industry, etc.…
Characteristics: Medium chemical resistance, Medium heat resistance; Resilient.

Reactivity at 25°C, with 1.8% of MEKP-925

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 16000 - 19000 cPRVF #4 Spindle @ 4 rpm
 
Processing PropertiesOriginal ValueComments
Gel Time 11.0 - 14.0 min
 
Descriptive Properties
Thixotropic Index5.5-6.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9184 / 231779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.