MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SCG Chemicals S11 Linear low density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: SCG S11 is a color compound linear low density polyethylene specifically developed for rotational molding applications. With a balance of stiffness and toughness, a large processing window and a wide variety of color selection, S11 is suitable for kayaks, water tanks, playground equipment, and other general rotomoulded articles.

Applications: Kayaks, Water storage tanks (<5000 L), Lawn and garden articles, Material handling containers, Pallets and bins, Automotive articles.

Features: Fast cooking. High stiffness. Good impact strength. Excellent color fastness and UV protection (UV8) for outdoor use. Wide variety of colors.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D 1505
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 18.0 MPa2610 psiCrosshead speed 50 mm/min.; ASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiCrosshead speed 50 mm/min.; ASTM D638
Elongation at Break 800 %800 %Crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 0.700 GPa102 ksiASTM D790
Impact 27
@Thickness 5.50 mm,
Temperature -40.0 °C
27
@Thickness 0.217 in,
Temperature -40.0 °F
J/mm ARM Method, rotomolded
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM D2117
Crystallization Temperature 113 °C235 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C149 °FASTM D648
Vicat Softening Point 116 °C241 °FASTM D1525
 
Descriptive Properties
AppearanceBlack compound powder
 Colored compound powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC745 / 278002

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.