MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ZEON Zeotherm® 130-90B Thermoplastic Vulcanizate  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A high-performance thermoplastic vulcanizate (TPV) designed to survive long-term exposure to 150°C (300°F) air and oil. Ideal for automotive and industrial applications where there is exposure to heat and/or oil.

Optimized for blow-molded air duct applications.

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92After 168h, 150°C -- Air
 94After 168h, 150°C -- SF105 Oil
 95ASTM D2240
Tensile Strength at Break 1885 psiASTM D412
 1885 psiAfter 168h, 150°C -- Air
 2262 psiAfter 168h, 150°C -- SF105 Oil
Tensile Stress at Strain 1305 psi
@Strain 100 %
ASTM D412
Elongation at Break 165 %After 168h, 150°C -- Air
 180 %After 168h, 150°C -- SF105 Oil
 200 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -45.0 °CGehman T10; ASTM D1053
Brittleness Temperature -44.0 °CASTM D2137
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Geolast® 703-45 Thermoplastic Elastomer

PZEONC50 / 73109

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.