MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Nickel Alloy

Material Notes: Information supplied by Brush Wellman Engineered Materials.

Treatment required for max strength: 2.5 hrs @ 510ºC
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%
Stress Relaxation after 1000 hrs @ 200°C: 98%
Superficial Hardness: 15N 78-86

Brush Wellman's Alloy 360 beryllium nickel strip combines unique mechanical and physical properties required in today's high reliability electrical/electronic systems, heavy duty controls, electromechanical devices and in other high performance applications.

Properties of beryllium nickel Alloy 360 strip that a designer can use include ultimate tensile strength approaching 300,000 psi, yield strength up to 245,000 psi, excellent formability, stress relaxation less than 5% at 400°F, and fatigue strength (in reverse bending) of 85,000 - 90,000 psi at 10 million cycles.

Typically, this alloy is used for mechanical and electrical/electronic components that are subjected to elevated temperatures (up to 700°F for short times), and require good spring characteristics at these temperatures. Some applications for this alloy are thermostats, bellows, diaphragms, burn-in connectors, and sockets.

Rockwell Hardness 15N given as 78 - 86.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: UNS N03360
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.28 g/cc0.299 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 343 - 528343 - 528
Tensile Strength, Ultimate >= 1482 MPa>= 214900 psi
Tensile Strength, Yield >= 1034 MPa>= 150000 psi
Elongation at Break >= 12 %>= 12 %
Modulus of Elasticity 195 - 210 GPa28300 - 30500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.0000287 ohm-cm<= 0.0000287 ohm-cm>6% IACS conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 200 °C
7.78 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 48.0 W/m-K333 BTU-in/hr-ft²-°F
Melting Point 1195 - 1325 °C2183 - 2417 °F
Solidus 1195 °C2183 °F
Liquidus 1325 °C2417 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.85 - 2.05 %1.85 - 2.05 %
Copper, Cu <= 0.25 %<= 0.25 %
Nickel, Ni 97.3 %97.3 %as balance
Titanium, Ti 0.40 - 0.60 %0.40 - 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard
Materion Beryllium Nickel Strip - Alloy 360 Annealed
Brush Wellman Beryllium-Copper Alloy 171 1/4 HT (TH01) Temper
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated
Materion Beryllium Nickel Strip - Alloy 360 Hard

NBB204 / 15094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.