MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman EastaPure™ MPK  (discontinued **)
Categories: Other Engineering Material

Material Notes: CAS No. 107-87-9

Product Description: Eastman EastaPure™ MPK solvent is being offered for positive and negative photoresist formulations. It is a high-purity low-trace metal solvent and is tested to measure selected critical trace metals in parts-per-billion levels. EastaPure™ MPK can also be used in edge bead removal process after spin coating. The chemical substances for this product are listed as Inert Ingredients Permitted for Use in Nonfood Use Pesticide Products under the Federal Insecticide, Fungicide, and Rodenticide Act (FIFRA).

Application/Uses:

  • Advanced resist
  • Developers
  • Edge bead removal
  • Flat Panel/LCD
  • LED/OLED
  • Microelectronics
  • Negative tone resist
  • Photolithography
  • Photoresist
  • Photoresist stripper applications
  • Positive tone resist
  • Semiconductors
  • Solvents
Key Attributes:
  • Excellent resin solubility
  • High assay
  • High Purity/Low Trace Metals
  • Inert - Nonfood use

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.806 - 0.809 g/cc
Viscosity 0.68 cP
 0.70 cPLiquid
Molecular Weight 86.13 g/mol
Vapor Pressure 0.0366 atm
@Temperature 20.0 °C
 0.189 atm
@Temperature 55.0 °C
Surface Tension 26.6 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 36.5 atm
Critical Temperature 287.9 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
Melting Point -86.0 °CFreezing Point
Boiling Point 101 - 105 °C@ 760 mm Hg
Flash Point 8.00 °CTag Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.387 - 1.393
@Temperature 25.0 °C
 1.3902
@Temperature 20.0 °C
 
Descriptive Properties
ColorPT-Co
Upper Limits for Trace Metals20 ppbAluminum
 20 ppbBarium
 20 ppbCadmium
 20 ppbCalcium
 20 ppbChromium
 20 ppbCobalt
 20 ppbCopper
 20 ppbGallium
 20 ppbGermanium
 20 ppbIron
 20 ppbLead
 20 ppbLithium
 20 ppbMagnesium
 20 ppbManganese
 20 ppbNickel
 20 ppbPotassium
 20 ppbSilver
 20 ppbSodium
 20 ppbStrontium
 20 ppbTitanium
 20 ppbZinc

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5146 / 222340

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.