MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® OM-10250 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-10250 is designed for overmolding applications like grips and anti-skid parts for consumer/industrial products. Monprene OM-10250 a medium hardness, medium density, opaque grade that exhibits excellent adhesion to PC, ABS, and PC/ABS.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Filled; Light Stabilized; Low Flow; Medium Density; Medium Hardness; Lubricated; Slip; Sunlight Resistant; UV Absorbing

Uses: Appliances; Bonding; Cell Phones; Dental Applications; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Sporting Goods; Toothbrush Handles; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5454ASTM D2240
 50
@Time 5.00 sec
50
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 4.63 MPa672 psiDie C, 20 in/min, Flow; ASTM D412
 5.27 MPa764 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  1.98 MPa
@Strain 100 %
287 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 2.16 MPa
@Strain 100 %
314 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 3.17 MPa
@Strain 300 %
460 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 3.58 MPa
@Strain 300 %
519 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 520 %520 %Die C, 20 in/min, Flow; ASTM D412
 620 %620 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 26.8 kN/m153 pliDie C, 20 in/min, Flow; ASTM D624
 27.7 kN/m158 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set  25 %
@Temperature 22.8 °C,
Time 79200 sec
25 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 86 %
@Temperature 70.0 °C,
Time 79200 sec
86 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 138 - 188 °C280 - 370 °F
Middle Barrel Temperature 154 - 199 °C310 - 390 °F
Front Barrel Temperature 154 - 216 °C310 - 420 °F
Nozzle Temperature 154 - 221 °C310 - 430 °F
Melt Temperature 166 - 221 °C330 - 430 °F
Mold Temperature 10.0 - 32.2 °C50.0 - 90.0 °F
Drying Temperature 65.6 °C150 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 120 rpm50 - 120 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0896 / 237387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.