Polyvinyl Chloride Homopolymer having low molecular weight, is white and free-flowing resins produced by suspension polymerization process. The resin can easily blend with variety of additives to achieve desired qualities needed in many applications. Applications are ranging from general purpose to special products regarding customer's satisfactions. Applications: Pipe Fitting., Other Rigid Injection Products. Features: Excellent fusion property. Good initial coloration. Excellent thermal stability. Information provided by SCG. |