MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® RS LCFG3060 NC010 PA610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes:

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccDAM; ISO 1183
Water Absorption 3.3 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.40 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.014 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPaDAM; ISO 527-1/-2
Elongation at Break >= 50 %DAM; ISO 527-1/-2
Elongation at Yield 5.0 %DAM; ISO 527-1/-2
Tensile Modulus 1200 MPa50% RH; ISO 527-1/-2
 2000 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.40DAM; ISO 527-1/-2
 0.4450%RH; ISO 527-1/-2
Charpy Impact, Notched 6.80 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 8.70 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CInjection Optimum
 230 - 290 °CInjection
Mold Temperature 50.0 - 90.0 °CInjection
 70.0 °CInjection Optimum
Drying Temperature 80.0 °CExtrusion
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
 3.00 - 4.00 hourDehumidified Dryer; Extrusion
Moisture Content 0.060 %Extrusion
 0.10 %Injection
 
Descriptive Properties
Delivery formPellets
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking CodePA610ISO 11469
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Resin IdentificationPA610ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® 6129 NC010 PBT
DuPont Mobility and Materials Zytel® RS 3061HSL BK039A PA610
Envalior Akulon® K222-D Nylon 6 (European and Asian Grade) (Cond)
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
BASF Ultradur® B 2550 PBT

PZDSX5502 / 198142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.