MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon R37879X034 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.70 g/cc2.70 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 102 microns4.00 millayer 1; Arlon SQA-TMS-003
 305 microns12.0 millayer 2; Arlon SQA-TMS-003
 457 microns18.0 milsubstrate; Arlon SQA-TMS-003
 864 microns34.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777silicone property; ASTM D2240
Tensile Strength, Ultimate 4.72 MPa685 psisilicone property; ASTM D412
Elongation at Break 125 %125 %silicone property; ASTM D412
Adhesive Bond Strength 0.0155 MPa2.25 psiArlon SQA-TMS-011
Tear Strength 8.77 kN/m50.0 pliDie B; silicone property; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.7 kV/mm425 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.70 W/m-K11.8 BTU-in/hr-ft²-°Foverall; Arlon SQA-TMS-054
 1.40 W/m-K
@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F
@Temperature 212 °F
silicone property; ASTM E1530
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 7.22 °C
6.00 Month
@Temperature 45.0 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 10842S060 0.060" (1.52 mm) Fully Cured, Unsupported, Silicone Rubber
Rogers Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber
Rogers Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber
Rogers Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber

PARL062 / 79714

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.